Leave Your Message

China ASTM A350 LF1, LF2, LF3 Carbon/Alloy Steel Suppliers & Factory for Pipeline and Forged Flanges

GENERAL CHARACTERISTICS

Our high-quality steel grades, manufactured by leading China suppliers, are ideal for pipeline applications and the production of forged flanges. These versatile steels are engineered to withstand extreme temperatures, suitable for use down to –20ºF (LF1), –50ºF (LF2), and –150ºF (LF3). Partner with our experienced factory to ensure the reliability and performance of your projects.

    General Characteristics

    These grades of steel are used as pipeline steels and also in the production of forged flanges. They are suitable for use down to –20ºF (LF1,) –50ºF (LF2) and –150ºF (LF3.)

    Designation by Standards
    Mat. No. DIN EN AISI
    1.5622 14Ni6 - A350

    Chemical Analysis

    LF1
    C% Mn% Si% S% P% Cr% Ni%
    0.30 max 0.6/1.35 .15/.30 .040 max .035 max 0.30 max 0.40 max
    LF2
    C% Mn% Si% S% P% Cr% Ni%
    0.30 max 0.6/1.35 .15/.30 .040 max .035 max 0.30 max 0.40 max
    LF3
    C% Mn% Si% S% P% Cr% Ni%
    0.20 max 0.90 .20/.35 .040 max .035 max 0.30 max 3.3/3.7

    Applications

    These steels are primarily used for pipelines and forged flanges.

    Forging

    LF1 and LF2 grades would ideally be forged at around 2250-2300ºF(1230-1260ºC) and can’t be forged below 1650-1700ºF(900-925ºC.) The LF3 grade would be forged at around 2150-2200ºF (1175-1205ºC) and can’t be forged below 1700ºF (925ºC.)

    Welding / Heat Treatment

    Heat treatment of pipeline steels will no doubt be done on a continuous basis after welding. The structure of these steels will be initially determined by the rolling/forging process. The pipeline itself will be supplied from hot-rolled steels, the flanges etc. from forgings. The actual welding process will be primordial in ensuring the suitability and security of the pipeline and its subsequent performance. Preheat and post heat treatments are essential.

    The three grades listed here are easily weldable by all tried and tested methods.

    Machinability

    In the case of forged fittings and flanges, these grades can be machined as required, and ongoing experience will determine if machining is best done on an as-forged structure, a normalized structure or an annealed structure. In either case, in view of the critical nature of the end use, advice should be taken from a recognized heat treatment company.

    Frequently Asked Questions (FAQ)

    Q: What are the primary applications of LF1, LF2, and LF3 steel grades?
    These steel grades are primarily used as pipeline steels and for the production of forged flanges and fittings.
    Q: What are the low-temperature limits for LF1, LF2, and LF3?
    These grades are suitable for low-temperature service down to -20ºF for LF1, -50ºF for LF2, and -150ºF for LF3.
    Q: What is the equivalent standard designation for these steel grades?
    Under the standard designations, Material Number 1.5622 corresponds to DIN 14Ni6 and AISI A350.
    Q: What are the recommended forging temperatures for these steels?
    LF1 and LF2 should ideally be forged at 2250-2300ºF (1230-1260ºC) and not below 1650-1700ºF (900-925ºC). LF3 should be forged at 2150-2200ºF (1175-1205ºC) and not below 1700ºF (925ºC).
    Q: Are LF1, LF2, and LF3 steel grades weldable?
    Yes, all three grades are easily weldable by all tried and tested methods. However, preheat and post-heat treatments are essential to ensure pipeline performance and security.
    Q: How should the machining process for these forged fittings be determined?
    They can be machined as required. Ongoing experience will determine whether to machine them in an as-forged, normalized, or annealed state. Due to the critical nature of their end use, consulting a recognized heat treatment company is highly recommended.