GENERAL CHARACTERISTICS

Our steel grades are expertly manufactured as pipeline steels and are ideal for the production of forged flanges. These high-quality products are suitable for various applications, providing reliable performance in temperatures as low as –20ºF (LF1), –50ºF (LF2), and –150ºF (LF3). As a leading factory in China, we are committed to delivering superior steel solutions. Partner with us, the trusted suppliers of premium steel products.

    General Characteristics

    These grades of steel are used as pipeline steels and also in the production of forged flanges. They are suitable for use down to –20ºF (LF1), –50ºF (LF2) and –150ºF (LF3).

    Designation by Standards

    Mat. No. DIN EN AISI
    1.5622 14Ni6 - A350

    Chemical Analysis

    LF1:

    C% Mn% Si% S% P% Cr% Ni%
    0.30 max 0.6/1.35 .15/.30 .040 max .035 max 0.30 max 0.40 max

    LF2:

    C% Mn% Si% S% P% Cr% Ni%
    0.30 max 0.6/1.35 .15/.30 .040 max .035 max 0.30 max 0.40 max

    LF3:

    C% Mn% Si% S% P% Cr% Ni%
    0.20 max 0.90 .20/.35 .040 max .035 max 0.30 max 3.3/3.7

    Applications

    These steels are primarily used for pipelines and forged flanges.

    Forging

    LF1 and LF2 grades would ideally be forged at around 2250-2300ºF (1230-1260ºC) and can’t be forged below 1650-1700ºF (900-925ºC.) The LF3 grade would be forged at around 2150-2200ºF (1175-1205ºC) and can’t be forged below 1700ºF (925ºC.)

    Welding / Heat Treatment

    Heat treatment of pipeline steels will no doubt be done on a continuous basis after welding. The structure of these steels will be initially determined by the rolling/forging process. The pipeline itself will be supplied from hot-rolled steels, the flanges etc. from forgings. The actual welding process will be primordial in ensuring the suitability and security of the pipeline and its subsequent performance. Preheat and post heat treatments are essential.

    The three grades listed here are easily weldable by all tried and tested methods.

    Machinability

    In the case of forged fittings and flanges, these grades can be machined as required, and ongoing experience will determine if machining is best done on an as-forged structure, a normalized structure or an annealed structure. In either case, in view of the critical nature of the end use, advice should be taken from a recognized heat treatment company.

    Frequently Asked Questions

    What are the primary applications for LF1, LF2, and LF3 steel grades?

    These steel grades are primarily used for pipelines and the production of forged flanges.

    What are the low-temperature limits for each of these steel grades?

    They are suitable for service down to –20ºF for LF1, –50ºF for LF2, and –150ºF for LF3.

    What are the recommended forging temperatures for LF1, LF2, and LF3?

    LF1 and LF2 grades should ideally be forged at around 2250-2300ºF (1230-1260ºC) and cannot be forged below 1650-1700ºF (900-925ºC). The LF3 grade is forged at 2150-2200ºF (1175-1205ºC) and cannot be forged below 1700ºF (925ºC).

    Are these steel grades easily weldable?

    Yes, all three grades are easily weldable by all tried and tested methods. However, preheat and post-heat treatments are essential to ensure the suitability and security of the pipeline.

    What is the standard designation for material number 1.5622?

    According to the standards, material number 1.5622 is designated as 14Ni6 under DIN standards and A350 under AISI standards.

    How should machining be approached for forged fittings and flanges?

    These grades can be machined as required. Ongoing experience will determine whether machining is best done on an as-forged, normalized, or annealed structure. Due to the critical nature of their end use, it is advised to consult a recognized heat treatment company.